Zinc Penetration and Its Interaction with Grain Boundaries in Quenched Steel

In This Article

Most Popular This Week

Casting Industry Income in Iranian Year ۱۴۰۵: Foundry Wages and Shop/Plant Profit

What Is White Cast Iron? ۳ Main Types, Properties, Uses, and Limits

Article Summary

This article reviews zinc penetration and grain-boundary embrittlement during welding of QP980 steel, with a focus on liquid metal embrittlement (LME) in zinc-coated high-strength steels and the role of Fe–Zn intermetallic compounds (IMCs).

Zinc Penetration and Its Interaction with Grain Boundaries in Quenched Steel

This article reviews zinc penetration and grain-boundary embrittlement during welding of QP980 steel, with a focus on liquid metal embrittlement (LME) in zinc-coated high-strength steels and the role of Fe–Zn intermetallic compounds (IMCs).

Abstract

Liquid metal embrittlement in zinc-coated high-strength steels is closely linked to the formation of Fe–Zn intermetallic compounds. The relationship between LME crack propagation and Fe–Zn IMC phases during resistance spot welding of galvanized QP980 steel was examined in a targeted study.

Results showed that in spot-welded galvanized QP980 joints, LME cracks form mainly at the weld center (Type I cracks) and at the weld shoulders (Type II cracks). The longest Type I crack was about 1014.8 μm, and the longest Type II crack was about 95.7 μm. Microstructural details and elemental distribution near LME cracks were also analyzed. Fe–Zn intermetallic compounds were identified along grain boundaries, which acted as preferential crack paths. Brittle IMCs can weaken the grain boundaries of the steel substrate and thereby promote initiation and further propagation of LME cracks.

Background: QP980 and Resistance Spot Welding

Advanced high-strength steel (AHSS) grade QP980 is a promising material for vehicles that must combine higher safety, environmental performance, and better energy efficiency with simultaneous strength and low weight. High-strength steel sheets are commonly supplied with a double-sided zinc-based coating for corrosion protection.

Resistance spot welding (RSW) is widely used on automotive assembly lines because of its high productivity, reliability, and process stability. However, liquid metal embrittlement cracks can form in galvanized QP980 during RSW and may severely degrade mechanical performance.

RSW involves rapid heating and cooling cycles. Welding parameters—including pulse number, current, and pulse schedule—affect microstructural evolution, residual stress, joint mechanical behavior, and especially LME formation.

Findings from Related Welding Studies

Sawanishi et al. and Eftekhari Melani et al. examined mechanical properties and microstructure of AHSS welded with pulsed resistance welding and reported fully martensitic microstructures for both single- and multi-pulse welds, with no significant change in microhardness.

Chabak et al. showed that dual-pulse welds develop finer prior-austenite grains and martensite packets in the coarse-grained heat-affected zone compared with single-pulse welds. Improved cross-tension strength and energy absorption of dual-pulse welds may be linked to lower residual stress. The weld edge and a large fraction of high-angle grain boundaries in the coarse-grained HAZ can act as barriers to crack initiation and growth.

Similarly, Wintjes et al. reported that multi-pulse current schedules can successfully reduce LME. Even so, parameter adjustments alone only reduce LME to a limited extent, and LME initiation remains a debated issue.

Zinc Melting and Grain-Boundary Penetration

Zinc melts at about 420 °C, while the iron substrate remains solid. Liquid zinc can then contact the steel and, under certain conditions, penetrate the solid metal and form LME cracks. Studies show that intergranular crack propagation is a characteristic feature of LME cracks in high-strength steels and is associated with the presence of zinc.

Understanding zinc–grain-boundary interaction is therefore essential for welding process control of quenched and partitioned steels such as QP980. At Taimaz Foolad (Metco), metallurgical insight into coating–substrate behavior supports better material selection and welding-related risk assessment for industrial steel applications.

Leave a Comment

Your email address will not be published. Required fields are marked *

Related Articles

Shopping Cart

ارسال مشخصات قطعه

مشخصات، نقشه یا تصویر قطعه را ارسال کنید تا کارشناسان تایماز فولاد با شما تماس بگیرند.

    افزودن نقشه، تصویر یا فایل قطعه

    فایل یا تصویر خود را انتخاب کنید یا بکشید و در این قسمت رها کنید.

    JPG, PNG, PDF, DWG, STEP

    Scroll to Top

    ارسال مشخصات قطعه

    مشخصات، نقشه یا تصویر قطعه را ارسال کنید تا کارشناسان تایماز فولاد با شما تماس بگیرند.

      افزودن نقشه، تصویر یا فایل قطعه

      فایل یا تصویر خود را انتخاب کنید یا بکشید و در این قسمت رها کنید.

      JPG, PNG, PDF, DWG, STEP